Brand Name : KAIXIN
Model Number : KX-Alloy HIP22
Certification : ISO9001:2015
Place of Origin : China
MOQ : 200KG
Price : To negotiate
Payment Terms : T/T, L/C
Supply Ability : 50~80 TONS per MONTH
Delivery Time : 45~60days
Packaging Details : Wooden Box, size as per guests' request
Shape : Wire,Strip,Rod,Tube,Plate
Alloy type : Soft Magnetic Alloy
Raw Materials : NI49-51%,V 0.8-1.8%,Fe Rem
Executive standard : ASTM
Delivery State : Sosoloid
Application : Suitable for light weight and small size electrical components for aviation and aerospace applications, such as microelectronic rotor, electromagnet pole head, relay, transducer and etc.
Features : It has high saturation magnetic induction intensity, high Curie point and can maintain good magnetic stability at high temperature.
Size : Negotiable
KX Hiperco 50 Soft Magnetic Materials Soft Iron Light Rod On Soft Magnetic Alloy
Product Description and Application
Hiperco 50 is also known as Hiperco 50,AFK502,Supermendur, 1J22 iron cobalt alloy
Hiperco 50 has high saturation magnetic induction, which is suitable for manufacturing aircraft and instrument components requiring small volume and light weight. Among the existing soft magnetic materials, it has the highest saturation magnetic induction intensity (2.4T), the Curie point is also high (980℃) and the saturation magnetostriction coefficient (60 ~ 100×10-6) is the maximal. Because of the high saturation magnetic induction intensity, it can can greatly reduce the volume when produce the same power of the motor and can create a large suction force when making an electromagnet in the same cross-sectional area . Because of the high Curie point, the alloy can work at higher temperatures where other soft magnetic materials have been completely demagnetized and maintain good magnetic stability
Process Performance and Requirements
Vacuum Induction Furnace(VIM) and Electroslag Remelting Furnace(ESR)
Grade | Chemical Composition (Mass Fraction)(%) | |||||||||
C≤ | Mn≤ | Si≤ | P≤ | S≤ | Cu≤ | Ni≤ | Co | V | Fe | |
Hiperco 50 | 0.04 | 0.3 | 0.3 | 0.02 | 0.02 | 0.2 | 0.5 | 49.0~51.0 | 0.80~1.80 | Rem |
Grade | Resistivity/(μΩ·m) | Density/(g/cm3) | Curie Point/°C | Saturation Magnetostriction Coefficient/(×10-6) | Tensile Strength/MPa | |
Cold Hard State | Soft State | |||||
Hiperco 50 | 0.4 | 8.2 | 980 | 60~100 | 1325 | 490 |
Grade | Variety | Magnetic Induction Intensity /T≥ at Different Magnetic Field Intensities (A/m) | Coercive Force Hc/(A/m)≤ | |||||
B400 | B800 | B1600 | B2400 | B4000 | B8000 | |||
Hiperco 50 | Cold Rolled Strip | 1.6 | 1.8 | 2 | 2.1 | 2.15 | 2.2 | 128 |
Wire,Forging,Rolling | - | - | - | 2.05 | 2.15 | 2.2 | 144 |
Professional Customization
Cold-drawn Wire | ¢0.3~¢18mm(Delivery in rolls or trays) |
Hot-Rolling Wire | ¢5.5~¢20mm(Delivery in rolls) |
Strip | thickness 0.1~4.5*width 6~350mm(Supply in rolls or straight strips) |
Smooth Forged Rod on a Lathe | ¢60~350mm,L800-2500mm |
Hot-rolled Burnishing | ¢20~80mm,L1000-5000mm |
Cold Drawn and Burnishing | ¢2.5~18mm,L1000-8000mm |
Seamless Tube | ¢1~275mm,wall thickness 0.2~30,L1000-8000mm |
![]() |
Hiperco 50 Soft Magnetic Alloy ASTM Rod / Tube / Plate / Wire / Strip Images |